| Coating grade | Steel | Stainless steel | Cast iron | Non-ferrous metals / non-metals | High-temperature resistent alloys | Hardened materials |
| P40 PATM | P 1: 427 - 984 2: 0.010 - 0.047 3: 0.002 - 0.030 | - | S 1: 394 - 820 2: 0.008 - 0.043 3: 0.002 - 0.028 | - | - | - |
| P40 PPGO | P 1: 328 - 656 2: 0.012 - 0.047 3: 0.004 - 0.030 | - | S 1: 361 - 492 2: 0.010 - 0.043 3: 0.004 - 0.028 | - | - | - |
| K10 PPTi | S 1: 295 - 689 2: 0.012 - 0.047 3: 0.004 - 0.030 | - | P 1: 394 - 886 2: 0.012 - 0.047 3: 0.004 - 0.030 | - | - | S 1: 262 - 591 2: 0.004 - 0.039 3: 0.004 - 0.024 |
| M40 PPST | S 1: 262 - 656 2: 0.010 - 0.039 3: 0.002 - 0.024 | P 1: 262 - 689 2: 0.010 - 0.039 3: 0.002 - 0.024 | - | - | P 1: 98 - 295 2: 0.006 - 0.030 3: 0.002 - 0.024 | - |
P: primary application | S: secondary application
1: spindle speed (SFM in feet per minute) | 2: feed rate (IPT in inches) | 3: depth of cut (DOC in inches)